CHANGES IN THE STRUCTURE OF THE CERAMICS SURFACE UNDER THE INFLUENCE OF HYDROFLUOROUS ACID
https://doi.org/10.31143/2221-7789-2024-4-67-71
EDN: TASCLA
Abstract
The surface of the ceramic material was treated with a 10 % solution of hydrofluoric acid. It was shown that hydrofluoric acid actively reacts with the main components of the ceramic material to form various soluble and slightly soluble compounds. The use of ultrasonic vibrations allows increasing the solubility of poorly soluble compounds. A significant change in the morphology of the ceramic workpiece surface was found when it was treated with hydrofluoric acid. At the same time, the depth and nature of these changes significantly depend on the treatment time.
About the Authors
A. Kh. TeuvazhukovRussian Federation
A. N. Pshenokov
Russian Federation
T. A. Borukaev
Russian Federation
References
1. Вартанов Т.О. Сравнительная характеристика материалов, применяемых для изготовления безметалловых конструкций в стоматологии // Байкальский медицинский журнал. 2012. Т. 110,
2. № 3. С. 12–14.
3. Верещагин В.И., Хабас Т.А., Кулинич Е.А., Игнатов В.П. Керамические и стеклокерамические материалы для медицины: учебник. Томск: Издательство ТПУ, 2008. 151 с.
4. Ульянов Ю.А., Зарипова Э.М., Мингазова Э.Н. К вопросу о биосовместимости керамических имплантатов при оказании ортопедической помощи // Менеджер здравоохранения. 2023. № 9. С. 18–22.
5. Севбитов А.В., Дорофеев А.Е., Ершов К.А., Енина Ю.И., Калиновский С.И., Пустохина И.Г. Оценка влияния среды полости рта на прочностные характеристики эндокоронок из гибридной керамики в лабораторных условиях // Вестник ВолГМУ. 2020. Т. 4, № 76. С. 62–64.
6. Ермак Е.Ю., Долгих И.М., Парилов В.В. Результаты клинического исследования функционирования двух цельнокерамических систем накладок // Бюллетень ВСНЦ СО РАН. 2006. Т. 48, № 2. С. 170–173.
7. Dikicier S., Korkmaz C., Atay A. Surface roughness and characteristics of CAD/CAM zirconia and glass ceramics after combined treatment procedures // BMC Oral. Health. 2022. V. 22, N 524. P. 772.
8. Matinlinna J., Ying Kei Lung C., Kit Hon Tsoi J. Silane adhesion mechanism in dental applications and surface treatments: A review // Dent. Mater. 2018. V. 34, N 1. Р. 13–28.
9. Bajraktarova-Valjakova E., Grozdanov A., Guguvcevski L., Korunoska-Stevkovska V., Kapu- sevska B., Gigovski N., Mijoska A., Bajrak-tarova-Misevska C. Acid Etching as Surface Treatment Method for Luting of Glass-Ceramic Restorations, part 1: Acids, Application Protocol and Etching Effec- tiveness // J. Med. Sci. 2018. V. 3, N 6. Р. 568–573.
10. Антонова И.Н., Никитин В.С., Полтавец О.С. Цельнокерамические материалы для стоматологической практики: аналитический обзор в соответствии с новой классификацией // Институт Сто- матологии. 2020. Т. 88, № 3. С. 84–86.
11. Шацкая В.А., Шитиков Е.С., Бардушкин В.В. Особенности активации воды воздействием ультра- звука для разработки полимерно-строительных материалов // Пластические массы. 2024. № 4. С. 38–40.
Review
For citations:
Teuvazhukov A.Kh., Pshenokov A.N., Borukaev T.A. CHANGES IN THE STRUCTURE OF THE CERAMICS SURFACE UNDER THE INFLUENCE OF HYDROFLUOROUS ACID. Proceedings of the Kabardino-Balkarian State University. 2024;14(4):67-71. (In Russ.) https://doi.org/10.31143/2221-7789-2024-4-67-71. EDN: TASCLA
JATS XML